Description
The tip side of these probes is coated with polycrystalline diamond. The diamond lm is in-situ doped with boron to make it highly conducting. 1.6 spring constant is compatible for ResiScope & Soft ResiScope, conductive, PFM, KFM and EFM modes.
Tip Specifications | |
---|---|
Material | Si |
Shape | Rectangular |
Reflex Coating | Al / 50 nm |
Height (μm) | 14-16 |
Aspect Ratio | 1.5-3.0 |
ROC (nm) | 100-300 |
Coating | 100nm Doped Diamond |
Cantilever Specifications | ||||
---|---|---|---|---|
Spring Constant (N/m) | Frequency (kHZ) | Length (μm) | Width (μm) | Thickness (μm) |
3.0 | 62 | 225 | 30 | 3.0 |